I know... I have everything sitting in the garage ready to go...
New tip! My painter just picked up some new adhesion promoter - its made by SEM (so you know that **** is awesome). Its called *** Adhesion Promoter. He sprayed it on some spare shrouds I had, at the same time sprayed some of the Bully AP (another shroud). Painted both PXR (was painting that at the time). Let them sit for 3 days. I couldn't scrape the paint off of the shroud done with *** - the Bully stuff, fingernail and it was gone.
The only way to get that paint to chip was throwing the shroud in a pile of rocks. Or taking a screwdriver to it.
Only bad thing, it needs to sit and cure for about 3 days. He said after a day it was still "like normal" - fingernail against paint, came off. After 3, its solid. It also lays down a LOT smoother than any other AP he's used (even said it came out smooth from the aerosol can).
The first set of lights we are using it on..........well, lets just say its for a friend's dad - his F250. I can't wait to see those done, get me into the Ford game! LOL
(ok, sorry for the tangent!)